| ASTM or UL TEST |
PROPERTY |
UNFILLED |
| Physical |
| D570 |
Water Absorption (Saturation) (%) |
0.9 |
| D570 |
Water Absorption, 24 hrs (%) |
0.25 |
| Mechanical |
| D638 |
Tensile Strength (psi) |
10,000 |
| D638 |
Tensile Modulus (psi) |
450,000 |
| D638 |
Tensile Elongation at Break (%) |
60 |
| D790 |
Flexural Strength (psi) |
14,300 |
| D790 |
Flexural Modulus (psi) |
425,000 |
| D785 |
Hardness, Rockwell & Burnell |
R120 |
| Thermal |
| D696 |
Coefficient of Linear Thermal Expansion |
5.0 x 10 ^5 |
| D789 |
Melting Temp (˚F/˚C) |
347 |
| Electrical |
| D149 |
Dielectric Strength (V/mil) short time, 1/8"
thick |
380 |
| D150 |
Dielectric Constant at 1 MHz |
3.17 |